Could you pleasure share us visual inspection / acceptance criteria for welding procedure and welder qualification?

2 Likes

Visual inspection for the test coupon:

  • ASME IX: see QW-144 and QW-194
  • AWS D1.1: see 4.9.1 and 4.22.1

Acceptance criteria: see project specification and process application.
Read more: Type of test for welder qualification Test (ASME IX)